FLEETGUARD 弗列加滤芯 HF7094 HF7095 HF7097 HF7098 HF7100 HF7101 HF7102 HF7103 HF7104 HF7105 HF7106 HF7107 HF7108 HF7109 HF7110 HF7111 HF7304 HF7307 HF7314 HF7318 HF7319 HF7331 HF7332 HF7338 HF7339 HF7347 HF7351 HF7403 HF7404 HF7407 HF7408 HF7411 HF7442 HF7444 HF7448 HF7449 HF7450 HF7464 HF7451 HF7465 HF7467 HF7468 HF7470 HF7471 HF7472 HF7473 HF7474 HF7475 HF7476 HF7477 HF7478 HF7479 HF7480 HF7481 HF7482 HF7483 HF7487 HF7488 HF7489 HF7490 HF7491 HF7492 HF7493 HF7494 HF7495 HF7507 HF7508 HF7509 HF7510 HF7511 HF7512 HF7513 HF7514 HF7515 HF7516 HF7517 HF7518 HF7519 HF7520 HF7560 HF7701 HF7702 HF7703 HF7704 HF7705 HF7706 HF7716 HF7722 HF7723 HF7724 HF7725 HF7726 HF7727 HF7728 HF7729 HF7730 HF7731 HF7732 HF7733 HF7734 HF7735 HF7736 HF7737 HF7738 HF7739 HF7740 HF7749 HF7753 HF7759 HF7760 HF7764 HF7766 HF7767 HF7768 FLEETGUARD 弗列加滤芯 HF7769 HF7770 HF7771 HF7776 HF7780 HF7781 HF7782 HF7783 HF7784 HF7785 HF7786 HF7788 HF7789 HF7790 HF7791 HF7792 HF7793 HF7794 HF7795 HF7796 HF7807 HF7808 HF7809 HF7810 HF7811 HF7812 HF7813 HF7814 HF7815 HF7833 HF7834 HF7896 HF7901 HF7904 HF7905 HF7906 HF7907 HF7908 HF7909 HF7910 HF7911 HF7919
词条
词条说明
在钻孔灌注桩中,常埋设钢护筒来定位需要钻的桩位。护筒为钢护筒,壁厚10mm,护筒定位时,先以桩位中心为圆心,根据护筒半径在土上定出护筒位置,护筒就位后,施加压力将护筒埋入约50cm。如下压困难,可先将孔位处的土体挖出一部分,然后安放护筒埋入地下。在埋入过程中应检查护筒是否垂直,若发现偏斜,应及时纠正。陆上护筒埋放就位后,将护筒外侧用粘土回填压实,以防止护筒四周出现漏水现象,回填厚度约40-45cm
螺旋管加工焊接:焊接之前应彻底除掉有害于焊接的锈 、油、水份、油漆等,选定适合钢种的焊条。点焊时间距比碳钢点焊间距短,除掉焊渣时应使用螺旋管刷。焊完以后,为了防止局部腐蚀或强度下降,应对表面进行研磨处理或清洗。切断以及冲压:由于螺旋管比一般材料强度高,所以冲压以及剪切时需要更高的压力,而刀与刀间隙准确时才能不发生切变不良和加工硬化,最好采用等离子或激光切断,当不得不采用气割或电弧切断时,对热影响区
经有关对比试验,验证了螺旋管与直缝焊管的屈服压力与爆破压力实测值和理论值基本吻合,偏差接近。但无论是屈服压力还是爆破压力,螺旋管均低于直缝焊管。爆破试验还显示出螺旋管爆破口的环向变形率明显大于直缝焊管。由此证实,螺旋管的
输送管线由于输量的变化,在实际操作过程中,钢管是承受随机交变载荷的作用。了解钢管的低循环疲劳强度,对判断管线的使用寿命具有重要的意义。按测定结果,螺旋管的疲劳强度与无缝管和电阻焊管相同,试验的数据与无缝管和电阻管分布在同一区内,而比一般的埋弧直缝焊管要高。现场的可焊性主要是由钢管的材质和端口配合尺寸公差决定的。考虑到钢管安装施工的要求,钢管加工生产的连续性的和外形几何尺寸的一致性尤为重要。螺旋管